Stability of the microstructure and elevated-temperature mechanical properties of additively manufactured inconel 718 superalloy subjected to long-term in-service thermal cycling
- Post by: Mohammad Jahazi
- March 7, 2022
- Comments off
FAYED, Eslam M., BRAILOVSKI, Vladimir, JAHAZI, Mohammad, et al. Materials Science and Engineering: A, 2022, p. 142790.