Dissimilar linear friction welding of selective laser melted Inconel 718 to forged Ni-based superalloy AD730™: Evolution of strengthening phases
- Post by: Mohammad Jahazi
- March 8, 2022
- Comments off
Seyedmohammad Tabaie, Farhad Rézaï-Aria, Bertrand C.D. Flipo, Mohammad Jahazi
Journal of Materials Science & Technology, Volume 96, 10 January 2022, Pages 248-261
Click here to read the Research Article